CTE, linear -3.00 - 23.0 µm/m-°C
-1.67 - 12.8 µin/in-°F
Average value: 6.17 µm/m-°C Grade Count:5
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
CTE, linear 1.00 - 23.0 µm/m-°C
0.556 - 12.8 µin/in-°F
Average value: 5.74 µm/m-°C Grade Count:31
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
CTE, linear 23.0 - 23.0 µm/m-°C

@Temperature 140 - 180 °C
12.8 - 12.8 µin/in-°F

@Temperature 284 - 356 °F
Average value: 23.0 µm/m-°C Grade Count:2
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled