Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.2 µm/m-°C @Temperature 260 °C |
9.56 µin/in-°F @Temperature 500 °F |
|
Ferro EG 3608 Metal Sealing Glass Type: Si-Ti Alkali Typical Powder Form: VSD Typical Application: Al Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals fo.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 20.0 - 1000 °C |
9.56 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Goodfellow T1-Thermocouple Alloy The positive element of the type K thermocouple alloy the negative being T2. The thermocouple can be used up to 1250C in oxidizing atmospheres and is the probably the most common in use. It is also .. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TB Wire quenched Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TD2 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TD4 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TDX Rod quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TDX Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TH1 Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TH1 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TH2 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TH3 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TH4 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 THX Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 THX Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TD1 Rod quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TD1 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TD3 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
CTE, linear | 17.2 µm/m-°C @Temperature 0.000 - 200 °C |
9.56 µin/in-°F @Temperature 32.0 - 392 °F |
|
CLAL-MSX DECLAFOR® 1015 TF Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |