Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 108 µm/m-°C @Temperature -40.0 - 149 °C |
60.0 µin/in-°F @Temperature -40.0 - 300 °F |
TMA; ASTM E831 |
Quadrant EPP Proteus® LSG HS PP - Heat Stabilized Polypropylene (ASTM Product Data Sheet) |
|||
CTE, linear | 108 - 120 µm/m-°C | 60.0 - 66.7 µin/in-°F | Average value: 116 µm/m-°C Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |
|||
CTE, linear | 108 µm/m-°C @Temperature 100 °C |
60.0 µin/in-°F @Temperature 212 °F |
|
Greene Tweed ARâ„¢ 1 Abrasive-Resistant Thermoplastic Sand and other abrasives are often a challenge for pump users in the power industry. Clearances on line shaft bearings and bowl wear rings open up, increasing pump vibrations and reducing pump effi.. |
|||
CTE, linear | 108 µm/m-°C @Temperature 20.0 °C |
60.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Formalloy HG High-Gloss TPO Alloy Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
CTE, linear | 108 µm/m-°C @Temperature 20.0 °C |
60.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Formalloy LG Low-Gloss TPO Alloy Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
CTE, linear | 108 µm/m-°C @Temperature 20.0 °C |
60.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Polypro SP-1710 Co/Pol Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
CTE, linear | 108 µm/m-°C @Temperature 20.0 °C |
60.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech PolyTeak Low Stress HDPE Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
CTE, linear | 108 µm/m-°C @Temperature 20.0 °C |
60.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech SP-1010 Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
CTE, linear | 108 µm/m-°C | 60.0 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® H37-MPT Epoxy Material Description: A single component, silver-filled and electrically conductive adhesive designed for semiconductor die attach and bonding SMDs for hybrid microelectronic packaging. It is certi.. |
|||
CTE, linear | 108 µm/m-°C | 60.0 µin/in-°F | T>Tg; ASTM E831-93 |
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 500 System Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 500 system.All information provided by 3D Systems. |
|||
CTE, linear | 108 µm/m-°C @Temperature 20.0 °C |
60.0 µin/in-°F @Temperature 68.0 °F |
modified; ASTM D696 |
Solvay Engineered Polymers DEXFLEX® 880 TPO
(discontinued **) Description: DEXFLEX® 880 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact, good processabil.. |
|||
CTE, linear | 108 µm/m-°C @Temperature 20.0 °C |
60.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Soft Touch PPR Co-Extruded Polyolefin Skin/PPR Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |