Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 °C |
6.94 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® ULS-12HLG Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 °C |
6.94 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® ULS-12 Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 °C |
6.94 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® ULS-12LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An ultra low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices such as TSOPs and.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 100 °C |
6.94 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals BRIGHTRAY® Alloy B Electrical Resistance Alloy A nickel-iron-chromium electrical-resistance alloy for use at operating temperatures up to 2010°F (1100°C). It contains rare-earth additions for increased oxidation resistance, especially und.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 100 °C |
6.94 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals BRIGHTRAY® Alloy C Electrical Resistance Alloy A nickel-chromium electrical-resistance alloy for use at operating temperatures up to 2100°F (1150°C). It contains rare-earth additions for increased oxidation resistance, especially under co.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 500 °C |
6.94 µin/in-°F @Temperature 68.0 - 932 °F |
|
Special Metals BRIGHTRAY® Alloy S Electrical Resistance Alloy A nickel-chromium electrical-resistance alloy for use at temperatures up to 2100°F (1150°C) under continuous operating conditions. It is similar to BRIGHTRAY alloy C but does not contain rare.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 100 °C |
6.94 µin/in-°F @Temperature 68.0 - 212 °F |
|
Alloy Wire International RW 80 Ni-Cr Resistance Wire Used in heating elements and control resistors because of its electrical properties and resistance to oxidation under temperature cycling and frequent switching. Also used in hot cutting operations.. |