Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 52.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 93.6 µm/m-°C

@Temperature -40.0 - 176 °C
52.0 µin/in-°F

@Temperature -40.0 - 349 °F
ASTM D696
Ravago Manufacturing Americas Hylac® GP74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
CTE, linear 93.6 µm/m-°C

@Temperature 20.0 °C
52.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Acrylloy F Acrylic Sheet
Description: Acrylic SheetInformation provided by Spartech.
CTE, linear 93.6 µm/m-°C

@Temperature 20.0 °C
52.0 µin/in-°F

@Temperature 68.0 °F
Trelleborg Sealing Solutions Turcite® TA Self-Lubricating Thermoplastic Rod
Turquoise color. Turcite® TA was developed for general purpose load and speed applications. It exhibits an excellent surface finish when machined. It has exceptional service life and superior ch..
CTE, linear 93.6 µm/m-°C

@Temperature 20.0 °C
52.0 µin/in-°F

@Temperature 68.0 °F
Trelleborg Sealing Solutions Turcite® TX Self-Lubricating Thermoplastic Rod
Red color. Turcite® TX is engineered to handle moderate load, high speed applications. It exhibits an excellent surface finish when machined. It has a long service life and exceptionally low coe..
CTE, linear 93.6 µm/m-°C
52.0 µin/in-°F
Average value: 93.6 µm/m-°C Grade Count:6
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..
CTE, linear 93.6 - 93.6 µm/m-°C

@Temperature 0.000 - 100 °C
52.0 - 52.0 µin/in-°F

@Temperature 32.0 - 212 °F
Average value: 93.6 µm/m-°C Grade Count:3
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..
CTE, linear 93.6 µm/m-°C

@Temperature 20.0 °C
52.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
DuPont Surlyn® SURSG201UG  (discontinued **)
Surlyn Reflections® SG201UG is a modified ionomer resin for applications that require a high gloss, molded in color surface finish directly from the mold. The material is weatherable, durable and p..
Copyright © lookpolymers.com All Rights Reserved