Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.70 µm/m-°C @Temperature 20.0 °C |
5.39 µin/in-°F @Temperature 68.0 °F |
Longitudinal; ASTM E228 |
Polystrand ThermoPro™ IE6010 Unitape Unidirectional Polypropylene-Glass Composite Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer .. |
|||
CTE, linear | 9.70 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
5.39 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP511ES Glass Epoxy Laminate Description: NP511ES is a woven glass fabric with high temperature, static dissipative epoxy resin. It has excellent mechanical strength and electrical properties at elevated temperatures with a con.. |
|||
CTE, linear | 9.70 µm/m-°C @Temperature 20.0 - 300 °C |
5.39 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8405 UV-transmitting Glass Sodium-potassium-barium-silicate glass, highly UV-transmitting Used as envelope for germicidal lamps (low-pressure mercury vapor discharge lamps) and for UV detectors The heavy metal content for t.. |
|||
CTE, linear | 9.70 µm/m-°C @Temperature 20.0 °C |
5.39 µin/in-°F @Temperature 68.0 °F |
|
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4984 High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4984.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi.. |
|||
CTE, linear | 9.70 µm/m-°C @Temperature 20.0 °C |
5.39 µin/in-°F @Temperature 68.0 °F |
|
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4987 High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4987.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi.. |
|||
CTE, linear | 9.70 µm/m-°C @Temperature 20.0 °C |
5.39 µin/in-°F @Temperature 68.0 °F |
|
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4986 High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4986.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi.. |