Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 84.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
46.7 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E831
DuPont Bexloy® AXW507NC010 Modified Ionomer Resin  (discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
CTE, linear 84.0 µm/m-°C

@Temperature 20.0 °C
46.7 µin/in-°F

@Temperature 68.0 °F
ISO 11359
LG Chemical HT-700 ABS, High Strength, High Scratch Resistance
Information Provided by LG Chem
CTE, linear 84.0 µm/m-°C

@Temperature 20.0 °C
46.7 µin/in-°F

@Temperature 68.0 °F
ISO 11359
LG Chemical PI-642 ABS, Fitting, High Strength
Information Provided by LG Chem
CTE, linear 84.0 µm/m-°C

@Temperature 20.0 °C
46.7 µin/in-°F

@Temperature 68.0 °F
Tra-Con Tra-Bond 642-1 Epoxy Adhesive
TRA-BOND 642-1 unfilled epoxy adhesive is designed to provide a long pot life and cure rapidly at elevated temperatures. Information provided by Tra-Con Inc.
CTE, linear 84.0 µm/m-°C
46.7 µin/in-°F
Absolute Drying; ASTM-D696
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..