Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.00 - 500 µm/m-°C @Temperature 55.0 - 250 °C |
4.44 - 278 µin/in-°F @Temperature 131 - 482 °F |
Average value: 161 µm/m-°C Grade Count:9 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
|
GBC L3 Steatite Ideal for high frequency, low loss, high voltage insulation. Much less expensive than alumina insulatorsApplications: resistor forms, surge arrestors, standoffs, spacers, and coil forms.Machinabili.. |
|||
CTE, linear | 8.00 - 10.0 µm/m-°C @Temperature 20.0 °C |
4.44 - 5.56 µin/in-°F @Temperature 68.0 °F |
|
MMCC Al/B4C Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 260 °C |
4.44 µin/in-°F @Temperature 500 °F |
|
Ferro IP 530 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
MD |
Toyobo TS401 PPS, 40% Glass Fiber Reinforced Key Feature: General Purpose Grade - balanced characteristics suitable for a broad range of uses.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a spec.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
|
Zircar Refractory Composites RS-202 Refractory Sheet ZRCI Refractory Sheet Type RS-202 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
CTE, linear | 8.00 µm/m-°C | 4.44 µin/in-°F | |
CoorsTek StatSafe™ ADC Static Dissipative Alumina Specialized StatSafe™ ESD-safe alumina combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffnes.. |
|||
CTE, linear | 8.00 - 10.0 µm/m-°C @Temperature 1000 °C |
4.44 - 5.56 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CSN-309N Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 8.00 - 10.0 µm/m-°C @Temperature 1000 °C |
4.44 - 5.56 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CSN-309NM,Body Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 8.00 µm/m-°C | 4.44 µin/in-°F | |
COI Ceramics Nextel™ AS-N610 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 50.0 - 150 °C |
4.44 µin/in-°F @Temperature 122 - 302 °F |
IPC TM-650 2.4.41 |
Arlon CLTE-XT High Precision Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
CTE, linear | 8.00 - 10.0 µm/m-°C @Temperature 50.0 - 150 °C |
4.44 - 5.56 µin/in-°F @Temperature 122 - 302 °F |
IPC TM-650 2.4.41 |
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/8" to 1" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 - 1000 °C |
4.44 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Anderman Ceramics EA998 Sintered Alumina, 99.8% High purity fully dense alumina (99.8%) with high temperature capability of 1750°C. Available in rod, tube, plate, crucibles, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 1.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 100 - 1100 °C |
4.44 µin/in-°F @Temperature 212 - 2010 °F |
|
3M Nextel™ DF-11 Woven Fabric 610 Information provided by 3M |
|||
CTE, linear | 8.00 µm/m-°C | 4.44 µin/in-°F | DIN EN 821-1 |
CeramTec 433 Alumina, 99.9% 433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A .. |