Thermal Properties Metric English Comments
CTE, linear 5.50 µm/m-°C
3.06 µin/in-°F
TMA
Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC
LYTEX 4182 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance..
CTE, linear 5.50 µm/m-°C

@Temperature 25.0 - 260 °C
3.06 µin/in-°F

@Temperature 77.0 - 500 °F
Ferro IX 2405 Dental Glass
Glass Type: Sr-Al-B-Si Typical Application: Phase Separated Glass Filler Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro ..
CTE, linear 5.50 µm/m-°C

@Temperature 25.0 - 260 °C
3.06 µin/in-°F

@Temperature 77.0 - 500 °F
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to..
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 - 750 °C
3.06 µin/in-°F

@Temperature 68.0 - 1380 °F
BS 1902: section 5.3: 1990
Skamol Group SUPER 1100 E Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 - 750 °C
3.06 µin/in-°F

@Temperature 68.0 - 1380 °F
BS 1902: section 5.3: 1990
Skamol Group SUPER 1100 ET Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 - 750 °C
3.06 µin/in-°F

@Temperature 68.0 - 1380 °F
BS 1902: section 5.3: 1990
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
CTE, linear 5.50 µm/m-°C

@Temperature 1000 °C
3.06 µin/in-°F

@Temperature 1830 °F
Chosun Refractories AH-2 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.50 µm/m-°C

@Temperature 1000 °C
3.06 µin/in-°F

@Temperature 1830 °F
Chosun Refractories APB-4 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.50 µm/m-°C

@Temperature 1000 °C
3.06 µin/in-°F

@Temperature 1830 °F
Chosun Refractories IC-RK Special Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.50 µm/m-°C

@Temperature 1000 °C
3.06 µin/in-°F

@Temperature 1830 °F
Chosun Refractories IC-S Special Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.50 µm/m-°C

@Temperature 1000 °C
3.06 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SAL70 Special Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.50 µm/m-°C

@Temperature 1000 °C
3.06 µin/in-°F

@Temperature 1830 °F
Chosun Refractories AH-1 Acid-Proof and Heat-Resistant Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 - 1000 °C
3.06 µin/in-°F

@Temperature 68.0 - 1830 °F
Anderman Ceramics EM60 Mullite
Synthetic mullite available in rod, tube, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 19".Information provided by Anderman Ceramics.
CTE, linear 5.50 µm/m-°C

@Temperature 20.0 - 1000 °C
3.06 µin/in-°F

@Temperature 68.0 - 1830 °F
Ceradyne CeraTrex™ 146-12E Silicon Carbide
Features:corrosion resistancewear resistancetailored electrical propertiesApplications:semiconductor componentsInformation provided by Ceradyne Company