Thermal Properties Metric English Comments
CTE, linear 41.4 µm/m-°C
23.0 µin/in-°F
Average value: 41.4 µm/m-°C Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate ..
CTE, linear 41.4 µm/m-°C
23.0 µin/in-°F
CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic
HYTAC-FLX has been improved for optimum performance in transparent applications. The enhanced formulation is easy to polish and results in minimal to no scratches with transparent sheet materials. ..
CTE, linear 41.4 µm/m-°C

@Temperature 20.0 °C
23.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylene® P6-23FG-2600 23% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
CTE, linear 41.4 µm/m-°C

@Temperature 20.0 °C
23.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylon® NSG-240A-C 50% Ceramic and Glass Fiber Reinforced
Information provided by Asahi Thermofil
CTE, linear 41.4 µm/m-°C

@Temperature 20.0 °C
23.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylon® NSG-240A 50% Ceramic and Glass Fiber Reinforced
Information provided by Asahi Thermofil
CTE, linear 41.4 µm/m-°C

@Temperature 20.0 °C
23.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylon® NSG-240A-2H 50% Ceramic and Glass Fiber Reinforced
Information provided by Asahi Thermofil
CTE, linear 41.4 - 172 µm/m-°C
23.0 - 95.6 µin/in-°F
Average value: 67.7 µm/m-°C Grade Count:11
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
CTE, linear 41.4 µm/m-°C

@Temperature -40.0 - 149 °C
23.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho..
CTE, linear 41.4 µm/m-°C

@Temperature 20.0 °C
23.0 µin/in-°F

@Temperature 68.0 °F
ASTM D1525
PlastxWorld CEVIAN® S5220 20% GF PC/ABS alloy
Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld ..
Copyright © lookpolymers.com All Rights Reserved