Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.61 µm/m-°C @Temperature 20.0 - 400 °C |
2.56 µin/in-°F @Temperature 68.0 - 752 °F |
|
Hogen HM1100 Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers hig.. |
|||
CTE, linear | 4.60 µm/m-°C @Temperature 20.0 - 400 °C |
2.56 µin/in-°F @Temperature 68.0 - 752 °F |
|
Hogen HM3050 Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE.. |
|||
CTE, linear | 4.61 µm/m-°C @Temperature 20.0 - 400 °C |
2.56 µin/in-°F @Temperature 68.0 - 752 °F |
|
Mi-Tech Metals HD17D Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.Manufactured by powder metallurgy methods. The t.. |
|||
CTE, linear | 4.60 µm/m-°C @Temperature 20.0 - 400 °C |
2.56 µin/in-°F @Temperature 68.0 - 752 °F |
|
Mi-Tech Metals HD18D Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con.. |
|||
CTE, linear | 4.60 µm/m-°C @Temperature 20.0 - 300 °C |
2.56 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8447 Intermediate Sealing Glass Intermediate Sealing glass Sealing to the glasses 8449, 8486, 8412, 8250, 8245, and Kovar The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmIn.. |
|||
CTE, linear | 4.60 µm/m-°C @Temperature 20.0 - 300 °C |
2.56 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8252 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature applications in electrical engineering, for sealing to molybdenum, free from alkali Bulb and exhaust tube for halogen lamps for automotive,.. |
|||
CTE, linear | 4.60 - 5.00 µm/m-°C @Temperature 20.0 - 1000 °C |
2.56 - 2.78 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Goodfellow Tungsten Carbide/Cobalt Tungsten Carbide is a hard, brittle ceramic which, when combined with 6% to 10% Cobalt, forms a tough Cermet (Ceramic-Metal). This material was developed for use in cutting tools, having hard cerami.. |
|||
CTE, linear | 4.60 µm/m-°C @Temperature 25.0 - 1000 °C |
2.56 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM C372 |
CoorsTek Pure SiC™ HR CVD Silicon Carbide, > 99.9995% Data Provided by the manufacturer, CoorsTek, Inc. |
|||
CTE, linear | 4.60 µm/m-°C @Temperature 25.0 - 1000 °C |
2.56 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM C372 |
CoorsTek Pure SiC™ LR CVD Silicon Carbide, > 99.9995% Data Provided by the manufacturer, CoorsTek, Inc. |
|||
CTE, linear | 4.60 µm/m-°C @Temperature 0.000 - 300 °C |
2.56 µin/in-°F @Temperature 32.0 - 572 °F |
|
Corning 7059 Barium Borosilicate Glass Features a low alkali content of less than 0.3%. In thin sheet form, it is an ideal substrate glass that is also used for low-end LCD applications. Also available crushed/powdered for sealing and o.. |
|||
CTE, linear | 4.60 µm/m-°C @Temperature 1000 °C |
2.56 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SB75 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.60 µm/m-°C @Temperature 1000 °C |
2.56 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SSBN Tube Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.60 µm/m-°C | 2.56 µin/in-°F | Volumetric thermal expansion |
China-Yixing Longly Refractories ASM-125 Cordierite-Mullite Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b.. |