Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 26.6 µm/m-°C | 14.8 µin/in-°F | ASTM C531 |
Chesterton ARC NVE SYSTEM Vinyl Ester Lining Description: ARC NVE is a high performance, quartz reinforced, three-component, modified novolac vinyl ester lining capable of being applied to horizontal and vertical surfaces. The NVE system kit i.. |
|||
CTE, linear | 26.6 µm/m-°C | 14.8 µin/in-°F | |
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual .. |
|||
CTE, linear | 26.7 µm/m-°C | 14.8 µin/in-°F | |
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining.. |
|||
CTE, linear | 26.7 µm/m-°C | 14.8 µin/in-°F | |
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining.. |