Thermal Properties Metric English Comments
CTE, linear 2.90 µm/m-°C

@Temperature 20.0 °C
1.61 µin/in-°F

@Temperature 68.0 °F
MarkeTech Zinc Oxide (ZnO) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
CTE, linear 2.90 µm/m-°C

@Temperature 25.0 - 100 °C
1.61 µin/in-°F

@Temperature 77.0 - 212 °F
ASTM E831
M Cubed Technologies SSC-702 Reaction-Bonded Silicon Carbide
Medium-grained reaction-bonded SiC for high wear applications. Bullnoses, fan liners, hydrocyclone liners, etc. Can be cast into very large shapes (greater than 4 ft. square, 5-6 inches thick)Info..
CTE, linear 2.90 µm/m-°C

@Temperature 25.0 - 100 °C
1.61 µin/in-°F

@Temperature 77.0 - 212 °F
ASTM E831
M Cubed Technologies SSC-802 Reaction-Bonded Silicon Carbide
Medium-grained reaction-bonded SiC for high wear applications. Bullnoses, fan liners, hydrocyclone liners, etc. Can be cast into very large shapes (greater than 4 ft. square, 5-6 inches thick)Info..
CTE, linear 2.90 µm/m-°C

@Temperature 20.0 - 100 °C
1.61 µin/in-°F

@Temperature 68.0 - 212 °F
UCAR Carbon UCAR® CGW Isostatic Molded Graphite
Isostatically molded grade CGW is an ATJ-based material that has been processed to higher density and strength. Grade CGW is characterized by low permeability, erosion resistance and surface hardnes..
CTE, linear 2.90 µm/m-°C

@Temperature 20.0 °C
1.61 µin/in-°F

@Temperature 68.0 °F
Trelleborg Sealing Solutions HiMod® 924 Thermoplastic Bearing
Thermoplastic BearingCharacteristics: HiMod® 924 is a high temperature, high modulus material developed for those functions that require high strength and high compressive properties along with exc..
CTE, linear 2.90 µm/m-°C

@Temperature 20.0 - 650 °C
1.61 µin/in-°F

@Temperature 68.0 - 1200 °F
Du-Co Ceramics DC-65 Cordierite
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.