Material Notes:
Thermoplastic BearingCharacteristics: HiMod® 924 is a high temperature, high modulus material developed for those functions that require high strength and high compressive properties along with excellent chemical resistance and low thermal expansion. This compound is known for its high flexural modulus, high compressive strength, low thermal expansion, good chemical resistance, and low moisture absorption. It is also injection moldable.Applications: Valve seats, gas turbine engine and automotive under-hood components, sliding vanes, aerospace, and medicalInformation provided by Busak + Shamban, now Trelleborg Sealing Solutions.Busak+Shamban changed its name to Trelleborg Sealing Solutions in 2007.
Physical Properties Metric English Comments
Moisture Absorption at Equilibrium 0.050 %
0.050 %
Mechanical Properties Metric English Comments
Flexural Modulus 16.9 GPa
2450 ksi
Compressive Yield Strength 179 MPa
26000 psi
Thermal Properties Metric English Comments
CTE, linear 2.90 µm/m-°C

@Temperature 20.0 °C
1.61 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 260 °C
500 °F
Continuous
287.8 °C
550.0 °F
Intermittent