Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 60.0 - 400 µm/m-°C | 33.3 - 222 µin/in-°F | Average value: 117 µm/m-°C Grade Count:6 |
Overview of materials for PEN-PET This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent.. |
|||
CTE, linear | 13.0 - 400 µm/m-°C | 7.22 - 222 µin/in-°F | Average value: 60.2 µm/m-°C Grade Count:46 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
CTE, linear | 19.8 - 400 µm/m-°C | 11.0 - 222 µin/in-°F | Average value: 73.1 µm/m-°C Grade Count:13 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
CTE, linear | 350 - 400 µm/m-°C | 194 - 222 µin/in-°F | |
Master Bond MasterSil 153Med Silicone Paste for Medical Applications Description: Master Bond MasterSil 153Med is a two component silicone compound with a paste consistency for high performance bonding and sealing. It can be used for medical device applications as it.. |