Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.00 - 70.0 µm/m-°C | 4.44 - 38.9 µin/in-°F | Average value: 30.7 µm/m-°C Grade Count:10 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
|
GBC L3 Steatite Ideal for high frequency, low loss, high voltage insulation. Much less expensive than alumina insulatorsApplications: resistor forms, surge arrestors, standoffs, spacers, and coil forms.Machinabili.. |
|||
CTE, linear | 8.00 - 10.0 µm/m-°C @Temperature 20.0 °C |
4.44 - 5.56 µin/in-°F @Temperature 68.0 °F |
|
MMCC Al/B4C Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
CTE, linear | 8.00 - 10.0 µm/m-°C @Temperature 20.0 °C |
4.44 - 5.56 µin/in-°F @Temperature 68.0 °F |
|
MMCC Al/SiC Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
MD |
Toyobo TS401 PPS, 40% Glass Fiber Reinforced Key Feature: General Purpose Grade - balanced characteristics suitable for a broad range of uses.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a spec.. |
|||
CTE, linear | 8.00 µm/m-°C | 4.44 µin/in-°F | |
CoorsTek StatSafe™ ADC Static Dissipative Alumina Specialized StatSafe™ ESD-safe alumina combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffnes.. |
|||
CTE, linear | 8.00 - 10.0 µm/m-°C @Temperature 1000 °C |
4.44 - 5.56 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CSN-601N Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 8.00 µm/m-°C | 4.44 µin/in-°F | |
COI Ceramics Nextel™ AS-N610 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
CTE, linear | 8.00 µm/m-°C | 4.44 µin/in-°F | |
COI Ceramics Nextel™ AS-N650 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 50.0 - 150 °C |
4.44 µin/in-°F @Temperature 122 - 302 °F |
IPC TM-650 2.4.41 |
Arlon CLTE-AT Commercial Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-AT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 100 - 1100 °C |
4.44 µin/in-°F @Temperature 212 - 2010 °F |
|
3M Nextel™ 610 Composite Ceramic Fiber Chemical composition above is wt%. Filament diameter is 10-12 µm.3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 .. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/16" to 1/4" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/8" to 1" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 - 1000 °C |
4.44 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Anderman Ceramics EA998 Sintered Alumina, 99.8% High purity fully dense alumina (99.8%) with high temperature capability of 1750°C. Available in rod, tube, plate, crucibles, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 1.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 100 - 1100 °C |
4.44 µin/in-°F @Temperature 212 - 2010 °F |
|
3M Nextel™ DF-11 Woven Fabric 610 Information provided by 3M |
|||
CTE, linear | 8.00 - 81.0 µm/m-°C | 4.44 - 45.0 µin/in-°F | Average value: 52.4 µm/m-°C Grade Count:18 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 °C |
4.44 µin/in-°F @Temperature 68.0 °F |
|
Pyrotek ISOCAST Insulating Refractory Castable Pyrotek's Isocast is a refractory castable based on phosphate bonded calcium silicate material. Isocast exhibits excellent thermal insulation characteristics and very good behavior with respec.. |
|||
CTE, linear | 8.00 µm/m-°C @Temperature 20.0 - 1000 °C |
4.44 µin/in-°F @Temperature 68.0 - 1830 °F |
|
CeramTec 614/698 Alumina, 96% 614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink. |
|||
CTE, linear | 8.00 - 230 µm/m-°C | 4.44 - 128 µin/in-°F | Average value: 25.5 µm/m-°C Grade Count:49 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |