Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 77.4 µm/m-°C @Temperature 37.8 - 65.6 °C |
43.0 µin/in-°F @Temperature 100 - 150 °F |
ASTM D696 |
Fibre Glast 2000 / 2060 System 2000 Epoxy System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical .. |
|||
CTE, linear | 77.4 µm/m-°C @Temperature 20.0 °C |
43.0 µin/in-°F @Temperature 68.0 °F |
|
Aremco Aremco-Bond™ 2310 High Performance Epoxide Ceramic-Filled, 1:1, High Lap Shear and Peel Strength, Autoclavable. |
|||
CTE, linear | 77.4 µm/m-°C @Temperature 20.0 °C |
43.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 3020 Rigid PVC, Extrusion Georgia Gulf 3020 is a base for use of wood flour up to 40 percent. Impact strength and toughnessFlame retardantChemical resistanceDimensional stabilityInformation provided by Georgia GulfGeorgia G.. |