Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.40 µm/m-°C @Temperature 260 °C |
4.11 µin/in-°F @Temperature 500 °F |
Fired Thermal Expansion |
Ferro EG 2012 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |
|||
CTE, linear | 7.40 µm/m-°C @Temperature 20.0 °C |
4.11 µin/in-°F @Temperature 68.0 °F |
x-y direction |
MMCC Copper/Graphite Fiber GC 7-340 Metal Matrix Composite Discontinuous graphite fiber copper product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plated,.. |
|||
CTE, linear | 7.40 µm/m-°C @Temperature 25.0 - 600 °C |
4.11 µin/in-°F @Temperature 77.0 - 1110 °F |
|
ICE Al2O3 99.5 Data provided by the manufacturer, International Ceramic Engineering. |
|||
CTE, linear | 7.40 µm/m-°C @Temperature 25.0 - 600 °C |
4.11 µin/in-°F @Temperature 77.0 - 1110 °F |
|
ICE Al2O3 99.8 Data provided by the manufacturer, International Ceramic Engineering. |
|||
CTE, linear | 7.40 µm/m-°C @Temperature 1000 °C |
4.11 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SAL95S Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |