Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 64.1 µm/m-°C @Temperature -40.0 - 149 °C |
35.6 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products. |
|||
CTE, linear | 64.1 µm/m-°C | 35.6 µin/in-°F | |
BCC Products MB 4000 RED Urethane Foundry Plank MB4000 Red is an extremely tough, high impact Urethane Plank, that can replace aluminum and other metals for many foundry applications. Features: excellent machinability, low dust emission, mostly .. |
|||
CTE, linear | 64.1 µm/m-°C | 35.6 µin/in-°F | |
Atom Adhesives AA-BOND FS227 Epoxy Adhesive AA-BOND FS227 is a thixotropic polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wetting, toughness, a.. |