Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.30 µm/m-°C @Temperature 260 °C |
3.50 µin/in-°F @Temperature 500 °F |
|
Ferro EG 0026 Glaze and Sealant Glass Glass Type: Ca-B-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insul.. |
|||
CTE, linear | 6.30 µm/m-°C | 3.50 µin/in-°F | at Set Pt. |
Ferro EG 2778 Thick Film Glass Glass Type: Si-Al-Ca Typical Powder Form: MVG Typical Application: Dielectric Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct.. |
|||
CTE, linear | 6.30 - 7.00 µm/m-°C @Temperature 20.0 - 100 °C |
3.50 - 3.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
MarkeTech W85Cu Tungsten/Copper Heat Sink Material WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c.. |
|||
CTE, linear | 6.30 µm/m-°C @Temperature 20.0 °C |
3.50 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials Tantalum Carbide (TaC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
CTE, linear | 6.30 µm/m-°C @Temperature 1000 °C |
3.50 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories HL-18 Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 6.30 µm/m-°C | 3.50 µin/in-°F | |
COI Ceramics Nextel™ AS-N720 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
CTE, linear | 6.30 µm/m-°C @Temperature 20.0 - 1000 °C |
3.50 µin/in-°F @Temperature 68.0 - 1830 °F |
|
BNZ Materials BNZP-23 Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 6.30 µm/m-°C @Temperature 20.0 - 1000 °C |
3.50 µin/in-°F @Temperature 68.0 - 1830 °F |
|
BNZ Materials BNZP-23L Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 6.30 µm/m-°C @Temperature 20.0 - 1000 °C |
3.50 µin/in-°F @Temperature 68.0 - 1830 °F |
|
BNZ Materials BNZP-25L Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 6.30 µm/m-°C @Temperature 20.0 - 1000 °C |
3.50 µin/in-°F @Temperature 68.0 - 1830 °F |
|
BNZ Materials Color A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 6.30 µm/m-°C @Temperature 20.0 - 1000 °C |
3.50 µin/in-°F @Temperature 68.0 - 1830 °F |
|
BNZ Materials Color B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 6.30 µm/m-°C @Temperature 20.0 - 1000 °C |
3.50 µin/in-°F @Temperature 68.0 - 1830 °F |
|
BNZ Materials Color CA Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 6.30 µm/m-°C @Temperature 20.0 °C |
3.50 µin/in-°F @Temperature 68.0 °F |
|
Aremco AREMCOLOX™ 502-1400 (Bisque-fired) Machinable Alumina Good corrosion electrical and thermal shock resistance. Plates from 1/4" to 3/4" thick; rods from 1/4" to 3" diameter. Easily machined using conventional tools, no firing required. |
|||
CTE, linear | 6.30 µm/m-°C @Temperature 20.0 °C |
3.50 µin/in-°F @Temperature 68.0 °F |
|
Aremco AREMCOLOX™ 502-1400 (Full-Fired) Dense Alumina Parts fabricated to print. Excellent physical properties and corrosion resistance. For pump liners, nozzles, guides. Standard crucibles and bolts, nuts and washers from 4-40 to 1/4-20. |