Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.50 µm/m-°C | 3.06 µin/in-°F | TMA |
Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4182 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 25.0 - 260 °C |
3.06 µin/in-°F @Temperature 77.0 - 500 °F |
|
Ferro IX 2405 Dental Glass Glass Type: Sr-Al-B-Si Typical Application: Phase Separated Glass Filler Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro .. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 25.0 - 260 °C |
3.06 µin/in-°F @Temperature 77.0 - 500 °F |
|
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 - 750 °C |
3.06 µin/in-°F @Temperature 68.0 - 1380 °F |
BSÂ 1902: section 5.3: 1990 |
Skamol Group SUPER 1100 E Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 - 750 °C |
3.06 µin/in-°F @Temperature 68.0 - 1380 °F |
BSÂ 1902: section 5.3: 1990 |
Skamol Group SUPER 1100 ET Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 - 750 °C |
3.06 µin/in-°F @Temperature 68.0 - 1380 °F |
BSÂ 1902: section 5.3: 1990 |
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 1000 °C |
3.06 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories AH-2 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 1000 °C |
3.06 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories APB-4 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 1000 °C |
3.06 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories IC-RK Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 1000 °C |
3.06 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories IC-S Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 1000 °C |
3.06 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SAL70 Special Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 1000 °C |
3.06 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories AH-1 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 - 1000 °C |
3.06 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Anderman Ceramics EM60 Mullite Synthetic mullite available in rod, tube, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 19".Information provided by Anderman Ceramics. |
|||
CTE, linear | 5.50 µm/m-°C @Temperature 20.0 - 1000 °C |
3.06 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Ceradyne CeraTrex™ 146-12E Silicon Carbide Features:corrosion resistancewear resistancetailored electrical propertiesApplications:semiconductor componentsInformation provided by Ceradyne Company |