Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.70 - 150 µm/m-°C | 2.61 - 83.3 µin/in-°F | Average value: 51.6 µm/m-°C Grade Count:29 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 260 °C |
2.61 µin/in-°F @Temperature 500 °F |
|
Ferro F 2719 Metal Sealing Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Kovar Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals.. |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 20.0 - 300 °C |
2.61 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8240 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, free from alkali, blue colored, defined absorption Bulb and exhaust tube .. |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 20.0 - 300 °C |
2.61 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8242 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, low refractive index Clad tube for optical fibers, glass metal sealing The heavy metal content for the.. |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 20.0 - 300 °C |
2.61 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8253 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, for use at higher temperatures than glass 8252, free from alkali Bulb and.. |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 0.000 - 300 °C |
2.61 µin/in-°F @Temperature 32.0 - 572 °F |
|
Corning 7052 Alkali Barium Borosilicate Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated. |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 23.0 - 260 °C |
2.61 µin/in-°F @Temperature 73.4 - 500 °F |
ASTM D696 |
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Machined Parts High abrasion resistance, very low friction coefficient property, suitable for being applied to spin component of spin apparatusInformation provided by Daelim H&L |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 1000 °C |
2.61 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories HL-16 Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 1000 °C |
2.61 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SBSN-AN Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 1000 °C |
2.61 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SSBA Tube Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 20.0 - 1093 °C |
2.61 µin/in-°F @Temperature 68.0 - 1999 °F |
|
BNZ Materials C-22 Z Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 20.0 - 520 °C |
2.61 µin/in-°F @Temperature 68.0 - 968 °F |
|
Advanced Ceramics ACL 2088 Zinc Alumino-Silicate A low expansion glass-ceramic suitable for sealing to molybdenum.Information provided by Advanced Ceramics Limited (ACL) |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 27.0 - 175 °C |
2.61 µin/in-°F @Temperature 80.6 - 347 °F |
ASTM D696 |
3M 7959MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 27.0 - 175 °C |
2.61 µin/in-°F @Temperature 80.6 - 347 °F |
ASTM D696 |
3M 9059MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
CTE, linear | 4.70 µm/m-°C @Temperature 20.0 - 300 °C |
2.61 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8241 Alkaline Earth Aluminosilicate Glass Alkaline earth aluminosilicate glass for high temperature application in electrical engineering, for sealing to molybdenum, free from alkali, blue colored, defined absorption Bulb and exhaust tube .. |