Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 3.50 µm/m-°C @Temperature 23.0 - 260 °C |
1.94 µin/in-°F @Temperature 73.4 - 500 °F |
ASTM D696 |
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Direct Formed
(Unverified Data**) Information provided by Daelim H&L |
|||
CTE, linear | 3.50 µm/m-°C | 1.94 µin/in-°F | at Set Pt. |
Ferro EG 2790 Metal Sealing Glass Type: Si-B Typical Powder Form: VSD Typical Application: Si Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals for Kovar,.. |
|||
CTE, linear | 3.50 µm/m-°C @Temperature 260 °C |
1.94 µin/in-°F @Temperature 500 °F |
|
Ferro EG 2790 Metal Sealing Glass Type: Si-B Typical Powder Form: VSD Typical Application: Si Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals for Kovar,.. |
|||
CTE, linear | 3.50 µm/m-°C @Temperature 25.0 - 1000 °C |
1.94 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM C372 |
CoorsTek SC-BNL (SC-42) Loaded Reaction Bonded Silicon Carbide Thermal Shock Delta Tc = 137°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
CTE, linear | 3.50 µm/m-°C @Temperature 1000 °C |
1.94 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories BTCQ Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 3.50 µm/m-°C @Temperature 1000 °C |
1.94 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SBSN20 Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 3.50 µm/m-°C @Temperature 25.0 - 500 °C |
1.94 µin/in-°F @Temperature 77.0 - 932 °F |
|
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber Description: Manufactured near-oxygen-free using electron-beam curing. The fiber is homogeneously composed of ultrafine beta-SiC crystallites and carbon. The fiber has excellent strength and modulus.. |
|||
CTE, linear | 3.50 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
1.94 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |
|||
CTE, linear | 3.50 µm/m-°C @Temperature 20.0 - 500 °C |
1.94 µin/in-°F @Temperature 68.0 - 932 °F |
|
Zircar Ceramics ASH Alumina-Silica Insulation ZIRCAR Ceramics Alumina-Silica Insulation Type ASH is one of the first alumina-silica products produced by ZIRCAR. Made of bulk fiber and inorganic alumina binders Type ASH is uniform throughout its.. |