Thermal Properties Metric English Comments
CTE, linear 3.24 µm/m-°C

@Temperature 20.0 °C
1.80 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Owens Corning Glass Fiber Reinforced Nylon 6/6, 30 wt.% glass
Nylons, as a group, are inert to most organic solvents. They resist alkalis and salt solutions and they are attacked by strong mineral acids and oxidizing agents. Data provided by the manufacturer,..
CTE, linear 3.24 µm/m-°C

@Temperature 20.0 °C
1.80 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Owens Corning Glass Fiber Reinforced Polycarbonate, 10 wt.% glass
Data provided by the manufacturer, Owens Corning.
CTE, linear 3.24 µm/m-°C

@Temperature 20.0 °C
1.80 µin/in-°F

@Temperature 68.0 °F
Pyrotek Pyrocast ZR Refractory Shapes
Aggregate Base: Fused Silica / MulliteApplicationsTransfer troughs Information provided by Pyrotek.
CTE, linear 3.24 - 88.0 µm/m-°C
1.80 - 48.9 µin/in-°F
Average value: 40.3 µm/m-°C Grade Count:33
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
CTE, linear 3.24 - 5.66 µm/m-°C

@Temperature -60.0 - 60.0 °C
1.80 - 3.14 µin/in-°F

@Temperature -76.0 - 140 °F
perpendicular to c-axis
Mateck Sapphire (Al2O3)
Optical crystals