Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 167 µm/m-°C @Temperature -40.0 - 149 °C |
93.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet) |