Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 146 µm/m-°C @Temperature 20.0 °C |
81.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Clariflex® TFE/VF2/HFP Clariflex is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoro-propylene, and vinylidene fluoride. Notable properties include light transmission, chemical resistance.. |
|||
CTE, linear | 146 µm/m-°C @Temperature 20.0 °C |
81.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Propylux® Polypropylene Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance it abrasion. These properties makes it suitable f.. |
|||
CTE, linear | 146 µm/m-°C @Temperature 20.0 °C |
81.1 µin/in-°F @Temperature 68.0 °F |
|
Trelleborg Emerson & Cuming Stycast® XT-5038-9 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
CTE, linear | 146 µm/m-°C | 81.1 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 360T High Temperature Epoxy Material Description: A two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. It is a thixotropic.. |