Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.24 µm/m-°C @Temperature 0.000 - 20.0 °C |
7.356 µin/in-°F @Temperature 32.0 - 68.0 °F |
|
Mateck Quartz Crystalline (SiO2) Optical crystals |