Category | Ceramic , Oxide , Silicon Oxide |
Manufacturer | Mateck GmbH |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Mateck Quartz Crystalline (SiO2).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.649 g/cc @Temperature 20.0 °C |
0.09570 lb/in³ @Temperature 68.0 °F |
|
Solubility | 0.00 ppm | 0.00 ppm | |
a Lattice Constant | 4.9138 Ã… | 4.9138 Ã… | |
c Lattice Constant | 5.4052 Ã… | 5.4052 Ã… | |
Molecular Weight | 60.06 g/mol | 60.06 g/mol |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Vickers Microhardness | 9810 | 9810 | MPa |
Hardness, Mohs | 7.0 | 7.0 | |
Modulus of Elasticity | 87.0 GPa | 12600 ksi | no |
105 GPa | 15200 ksi | ne |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.24 µm/m-°C @Temperature 0.000 - 20.0 °C |
7.356 µin/in-°F @Temperature 32.0 - 68.0 °F |
|
Specific Heat Capacity | 0.741 J/g-°C | 0.177 BTU/lb-°F | |
Thermal Conductivity | 6.82 W/m-K @Temperature 25.0 °C |
47.3 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
11.43 W/m-K @Temperature 25.0 °C |
79.32 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
||
Melting Point | 1470 °C | 2680 °F |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Refractive Index | 1.5538 | 1.5538 | at n0.436 |
1.5632 | 1.5632 | at n0.436 | |
1.4996 @Wavelength 3000 nm |
1.4996 @Wavelength 3000 nm |
||
1.507 @Wavelength 3000 nm |
1.507 @Wavelength 3000 nm |
||
1.535 @Wavelength 1000 nm |
1.535 @Wavelength 1000 nm |
||
1.5438 @Wavelength 1000 nm |
1.5438 @Wavelength 1000 nm |
||
1.6493 @Wavelength 200.1 nm |
1.6493 @Wavelength 200.1 nm |
||
1.6623 @Wavelength 200.1 nm |
1.6623 @Wavelength 200.1 nm |
||
IR Transmittance | 10 % @Wavelength 4100 nm |
10 % @Wavelength 4100 nm |
Internal Transmittance |
80 % @Wavelength 3900 nm |
80 % @Wavelength 3900 nm |
Internal Transmittance | |
98 % @Wavelength 3000 nm |
98 % @Wavelength 3000 nm |
Internal Transmittance | |
UV Transmittance | 98 % @Wavelength 200 nm |
98 % @Wavelength 200 nm |
Internal Transmittance |
Descriptive Properties | Value | Comments |
---|---|---|
Symmetry Class | P321 | |
Syngony | hexagonal | |
Thermal Coefficient of Refractive Index | -3.93E-06 | ne at 340 nm for 20/100°C |
-5.01E-06 | no at 340 nm for 20/100°C | |
Transmission Range (microns) | 0.15 - 3.3 |