Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.7 µm/m-°C @Temperature 37.8 - 538 °C |
7.05 µin/in-°F @Temperature 100 - 1000 °F |
|
Meehanite GM-60 Flake Graphite Cast Iron Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a.. |
|||
CTE, linear | 12.7 µm/m-°C @Temperature 20.0 - 200 °C |
7.06 µin/in-°F @Temperature 68.0 - 392 °F |
|
Industeel CLC 1.2738 Prehardened Mold Steel (300HB/30HRC) for Thick Sections Description: CLC 1.2738 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, Nickel carbon and manganese additions are optimized to have a fully .. |
|||
CTE, linear | 12.7 µm/m-°C @Temperature 20.0 - 100 °C |
7.06 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals NIMONIC® Alloy 80A A nickel-chromium alloy similar to NIMONIC alloy 75 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good corrosion and oxidation resistance and high tensile a.. |
|||
CTE, linear | 12.7 µm/m-°C @Temperature 20.0 - 100 °C |
7.06 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals NIMONIC® Alloy 86 A nickel-chromium-molybdenum alloy with a rare-earth (cerium) addition. It combines good formability and weldability with exceptional resistance to oxidation and scaling at temperatures to 1920°.. |
|||
CTE, linear | 12.7 µm/m-°C @Temperature 20.0 - 100 °C |
7.06 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals NIMONIC® Alloy 90 A precipitation-hardenable nickel-chromium-cobalt alloy having high stress-rupture strength and creep resistance at temperatures to about 1700°F (920°C). The alloy also has good resistance to.. |
|||
CTE, linear | 12.7 µm/m-°C @Temperature 25.0 - 700 °C |
7.06 µin/in-°F @Temperature 77.0 - 1290 °F |
|
Du-Co Ceramics S-461 Magnesia Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
CTE, linear | 12.7 µm/m-°C @Temperature 20.0 - 100 °C |
7.06 µin/in-°F @Temperature 68.0 - 212 °F |
|
Alloy Wire International RW 118 Hot Cutting Wire - High Strength Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and for the heat sealing of polypropylene bags.Information provided by Alloywire International. |
|||
CTE, linear | 12.7 µm/m-°C @Temperature 20.0 - 200 °C |
7.06 µin/in-°F @Temperature 68.0 - 392 °F |
|
Assab Steels 618 Plastic Mold Material ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu.. |
|||
CTE, linear | 12.7 µm/m-°C @Temperature 20.0 - 200 °C |
7.06 µin/in-°F @Temperature 68.0 - 392 °F |
|
Assab Steels 718HH Plastic Mold Material IMPAX SUPREME is a premium-quality vacuum-degassed Cr-Ni-Mo-alloyed steel which is supplied in the hardened and tempered condition. IMPAX SUPREME is manufactured to consistently high quality standar.. |