Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 25.4 mm/min | 1.00 in/min | Pass: Burn Rate- Max 100; FMVSS 302 |
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Flame Spread | 25.4 mm/min | 1.00 in/min | Pass: Burn Rate- Max 100; FMVSS 302 |
Teknor Apex TEKRON® 4300-D88F Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Flame Spread | 25.4 mm/min | 1.00 in/min | Pass: Burn Rate- Max 100; FMVSS 302 |
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Flame Spread | 25.4 mm/min | 1.00 in/min | ASTM D635 |
DuPont™ Surlyn® 8660 Ionomer Resin, Sodium Surlyn® 8660 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Flame Spread | 25.4 mm/min | 1.00 in/min | ASTM D635 |
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit.. |
|||
Flame Spread | 25.4 mm/min | 1.00 in/min | ASTM D635 |
DuPont™ Surlyn® 9720 Ionomer Resin, Zinc Surlyn® 9720 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Flame Spread | 25.4 mm/min | 1.00 in/min | ASTM D635 |
DuPont™ Surlyn® 9721 Ionomer Resin, Zinc Surlyn® 9721 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |