Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 38 mm/min | 1.5 in/min | VSS-302 |
Multibase Multi-Flex® A 4001 LC Black TPE Thermoplastic Elastomer Features: Heat Resistance, HighOzone ResistantCompression Set, Low Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Flame Spread | 38 mm/min | 1.5 in/min | FMVSS302 |
Polyram Polytron P60B08-S Polypropylene, 60% Long Glass Fiber Polytron P60B08-S (Single strand) is a chemically coupled polypropylene 60% long glass fiber with extra load of additives for dilution.Information provided by Polyram. |
|||
Flame Spread | 38 mm/min @Thickness 1.00 mm |
1.5 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength stiffness and toughness excellent .. |