Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 37.0 - 54.0 mm/min | 1.46 - 2.13 in/min | Average value: 45.2 mm/min Grade Count:15 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |