Polymer Property : Flame Spread = 36 mm/min
Polymer Property :
Flame Spread =
36 mm/min
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Flame Spread
36
mm/min
1.4
in/min
Horizontal Burn Rate; FMVSS302
Asahi Kasei Thermylene® P6-30FG-0687 30% Glass Fiber Reinforced, Heat Stabilized