Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flame Spread = 25.4 mm/min Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flame Spread 25.4 mm/min
1.00 in/min
Pass: Burn Rate- Max 100; FMVSS 302
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer
Information provided by Teknor Apex Company
Flame Spread 25.4 mm/min
1.00 in/min
Pass: Burn Rate- Max 100; FMVSS 302
Teknor Apex TEKRON® 4300-D88F Thermoplastic Elastomer
Information provided by Teknor Apex Company
Flame Spread 25.4 mm/min
1.00 in/min
Pass: Burn Rate- Max 100; FMVSS 302
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer
Information provided by Teknor Apex Company
Flame Spread 25.4 mm/min
1.00 in/min
ASTM D635
DuPont™ Surlyn® 8660 Ionomer Resin, Sodium
Surlyn® 8660 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Flame Spread 25.4 mm/min
1.00 in/min
ASTM D635
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc
Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit..
Flame Spread 25.4 mm/min
1.00 in/min
ASTM D635
DuPont™ Surlyn® 9720 Ionomer Resin, Zinc
Surlyn® 9720 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Flame Spread 25.4 mm/min
1.00 in/min
ASTM D635
DuPont™ Surlyn® 9721 Ionomer Resin, Zinc
Surlyn® 9721 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..