Thermal Properties Metric English Comments
Decomposition Temperature 384 °C
723 °F
Degradation Temperature
Epoxy Technology EPO-TEK® 320 Optical, Opaque Epoxy
Product Description: EPO-TEK® 320 is a two component, black-colored and optically opaque epoxy designed for optical, medical, and optoelectronic packaging of semiconductor devices and components. ..
Decomposition Temperature 384 °C
723 °F
Degradation Temperature
Epoxy Technology EPO-TEK® H20F Electrically Conductive, Flexible Epoxy
Product Description: EPO-TEK® H20F is a two component, flexible silver epoxy. It was designed for flexible type circuitry, such as switching circuits in a flexible panel system, as well as large di..
Decomposition Temperature 384 °C
723 °F
Degradation Temperature
Epoxy Technology EPO-TEK® OG142-112 UV Cure Optical Epoxy
Material Description: Single component, medium viscosity, UV curable epoxy for adhesive sealing and encapsulating fiber optic and optoelectronic packaging application. Replacement version of EPO-TE..