Thermal Properties Metric English Comments
Decomposition Temperature 220 °C
428 °F
Average value: 220 °C Grade Count:26
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Decomposition Temperature >= 220 °C
>= 428 °F
Thermal Stability; ASTM D2513/D3350
Ineos TUB 121 HDPE
TUB 121 (aka ELTEX® TUB 121, ELTEX® TUB 121 N2025, and ELTEX® TUB 121 N3000) is a black high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, ind..
Decomposition Temperature >= 220 °C
>= 428 °F
Thermal Stability; ASTM D2513/D3350
Ineos TUB 121N HDPE
TUB121N is a natural high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, industrial, and mining pipe. When blended with an approved black concentrate, t..
Decomposition Temperature >= 220 °C
>= 428 °F
Thermal Stability; ASTM D2513/D3350
Ineos TUB 172 HDPE
TUB 172 is a yellow medium density polyethylene copolymer designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stress life and slow crack growth resistance. T..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Neopor® 2300 Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Neopor® 2400 Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Neopor® 5300 Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Neopor® 5300 Plus Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Peripor® 200 Expandable Polystyrene
Description: Expandable polystyrene (EPS) with uniformly distributed flame retardant (blowing agent: pentane)Remarks: Low-pentane products for the production of flame-retardant foams displaying low ..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® F 215 N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing a uniformly distributed ?ame retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foams.Applications: Blocks, insula..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® F 215 T-N Expandable Polystyrene
Use: Expanding-agent containing plastic for the production of foam plasticInformation provided by BASF
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® F 315 T-N Expandable Polystyrene
Use: Expanding-agent containing plastic for the production of foam plasticsInformation provided by BASF
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® F 315-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkageApplicati..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® F 395 -N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® F 415-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foamsApplications: Visible cover pa..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® P 326 M Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded parts with very good mechanical ..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® P 570 Expandable Polystyrene Additive
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: For the production of expanded particles as a filling material ..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Peripor® 300 Expandable Polystyrene
Description: Expandable polystyrene (EPS) with uniformly distributed flame retardant (blowing agent: pentane)Remarks: Low-pentane products for the production of flame-retardant foams displaying low ..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® F 215 L-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing a uniformly distributed came retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foams.Applications: Low-density bl..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® F 295-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkageApplicati..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® F 495-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® P 226 C Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Blocks with very short cycle times.Info..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® P 326 C Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded partsInformation provided by BAS..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® P 326 Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded partsInformation provided by BAS..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® P 426 Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts.Information pr..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® P 656 Expandable Polystyrene Additive
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: Filling material for lightweight plasters.Information provided ..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Neopor® 2200 Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Neopor® 2400 CT Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Neopor® P 5200 Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of silver-gray foams having a considerably higher ther..
Decomposition Temperature >= 220 °C
>= 428 °F
BASF Styropor® P 426 C Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts with very shor..