Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 74.0 °C | 165 °F | Tag Closed Cup |
LyondellBasell Glycol Ether EBA Ethylene glycol butyl ether acetate Information provided by Lyondell. |
|||
Flash Point | 74.0 °C | 165 °F | closed cup |
Dow Corning SYL-OFF® 7678 CROSSLINKER Syl-Off® 7678 Crosslinker is a 100% active solids silicone crosslinker. Recommended where optimum cure performance and bathlife are required. Suitable for use with Syl-Off® Solventless and Solvent.. |
|||
Flash Point | 74.0 °C | 165 °F | closed cup |
Dow Corning SYL-OFF® SL 7028 CROSSLINKER Solvent-free, but suitable for both solvent and solventless coatingInformation provided by Dow Corning |
|||
Flash Point | 74.0 °C | 165 °F | closed cup |
Dow Corning Z-6187 SILANE Dow Corning® Z-6187 Silane is a dialkyldimethoxysilane. Silanes and siloxanes have been used for some time in this application to increase yield and improve the stereoregularity of the polyolefin r.. |
|||
Flash Point | 74.0 °C | 165 °F | Open Cup |
3M CC-2 Cable Cleaning Preparation Kits 3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form.. |
|||
Flash Point | 74.0 °C | 165 °F | Open Cup |
3M CC-3 Cleaning Pad Kits 3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form.. |
|||
Flash Point | 74.0 °C | 165 °F | Open Cup |
3M CC-4 Cleaning Solvent 3M CC series Cable Cleaning Solvent is a full strength non-ozone depleting solvent cleaner, degreaser for use as an effective replacement for 1,1,1-Trichloroethane and other hazardous solvents, Form.. |
|||
Flash Point | 73.7 °C | 165 °F | |
BASF Piperazine 68% Formula: C4H10N2CAS: 110-85-0Description Piperazine 68% is a colorless to yellow hot molten with an amine-like odor. It is miscible in water.Synonyms: 1,4-Diazacyclohexane, 1,4-Piperazine, Hexahydr.. |