Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 56.0 °C | 133 °F | Tag Closed Cup |
LyondellBasell PMP Propylene glycol methyl ether propionate Information provided by Lyondell. |
|||
Flash Point | 56.1 °C | 133 °F | ASTM D56 |
ExxonMobil Isopar™ K (AM) Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation pr.. |
|||
Flash Point | 56.0 °C | 133 °F | |
BASF Formic Acid - 95% Formula: CH2O2CAS: 64-18-6Description: Formic Acid 95% is a colorless to yellowish liquid, with a pungent odor. It is miscible with water and other organic substances in all proportion.Synonyms: Me.. |
|||
Flash Point | >= 56.0 °C | >= 133 °F | Pensky a Martens |
Unipetrol PND 33-352-94 Extra Light Fuel Oil Extra light fuel oil si a mix of liquid hydrocarbons obtained from crude oil through distillation and other refining processes, boiling mostly within 150 to 370 °C. It may contain additives to lowe.. |