Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 238 °C | 460 °F | |
LG Chemical LGflex GL300 Plasticizer Features: Excellent Viscosity, Heat Stability and Non-endocrine disrupterApplication: PVC Calenderings/Leathers, Sheets, Gloves, HoseInformation provided by LG Chemical |
|||
Flash Point | 238 °C | 460 °F | |
Lubriplate AC-3 Petroleum-Based Air Compressor Fluid Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar.. |
|||
Flash Point | 238 °C | 460 °F | |
Lubriplate H0-3 Petroleum-Based Heavy-Duty Hydraulic Oil Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin.. |
|||
Flash Point | 238 °C | 460 °F | ASTM D92 |
ExxonMobil 680 Mobilgear SHC XMP Series Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin .. |
|||
Flash Point | 238 °C | 460 °F | ASTM D92 |
ExxonMobil 34 Mobil Mist Lube Series Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig.. |
|||
Flash Point | 238 °C | 460 °F | |
ConocoPhillips Syncon® 10W-30 High Performance Synthetic Motor Oil Description: Conoco Syncon HP Synthetic Motor Oil is formulated for most domestic or imported vehicles with gasoline-powered engines. It works well at extreme temperatures and in severe driving cond.. |
|||
Flash Point | 238 °C | 460 °F | |
ConocoPhillips Syncon® 15W-50 High Performance Synthetic Motor Oil Description: Conoco Syncon HP Synthetic Motor Oil is formulated for most domestic or imported vehicles with gasoline-powered engines. It works well at extreme temperatures and in severe driving cond.. |
|||
Flash Point | 238 °C | 460 °F | |
ConocoPhillips Syncon® EP Gear Oil, AGMA number 8EP Description: Conoco Syncon EMGARD EP Gear Oil 680 is specifically formulated to protect moderate to heavily loaded industrial gears and bearings. It provides excellent antiwear and load-carrying cap.. |
|||
Flash Point | 238 °C | 460 °F | Base Oil Property |
ConocoPhillips Syncon® Extra Long Life Grease NLGI No. 00 Description: Conoco Syncon Extra Long Life Grease is an ultra high performance lithium-complex grease with heavy synthetic base oil specifically designed for long service life under heavily loaded c.. |
|||
Flash Point | 238 °C | 460 °F | ASTM D92 |
ChevronTexaco Delo® 400 SAE 20 Chevron Delo 400 heavy duty motor oils are exceptional, super premium quality “universal” engine oils which exceed industry and engine manufacturers’ performance requirements.They are formulated .. |
|||
Flash Point | 238 °C | 460 °F | ASTM D92 |
ChevronTexaco ISO 460 Synthetic Wheel Motor Lubricant EP FeaturesChevron Synthetic Wheel Motor Lubricants EP are superior quality industrial EP gear lubricants. Their advanced formulation provides superior load carrying and antiwear properties; protection.. |
|||
Flash Point | 238 °C | 460 °F | ASTM D92 |
ChevronTexaco ISO 680 Synthetic Wheel Motor Lubricant EP FeaturesChevron Synthetic Wheel Motor Lubricants EP are superior quality industrial EP gear lubricants. Their advanced formulation provides superior load carrying and antiwear properties; protection.. |
|||
Flash Point | 238 °C | 460 °F | PMCC; ASTM D92 |
ExxonMobil Exterex™ A32 Synthetic Fluid Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol.. |
|||
Flash Point | 238 °C | 460 °F | |
ChevronTexaco Pinnacle® EP 320 Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe.. |
|||
Flash Point | 238 °C | 460 °F | ASTM D92 |
ChevronTexaco RPM® SAE 15W-40 Heavy Duty Motor Oil Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha.. |
|||
Flash Point | 238 °C | 460 °F | ASTM D92 |
ChevronTexaco Supreme SAE 5W-20 Motor Oil FeaturesChevron Supreme Motor Oils are premium quality automotive engine oils.Chevron Supreme Motor Oils SAE 5W-20, 5W-30, 10W-30, 10W-40, and 20W-50 are formulated with ISO-SYN™ base stocks, a she.. |
|||
Flash Point | 238 °C | 460 °F | |
ChevronTexaco URSA® SAE 15W-40 Super Plus Texaco Ursa Super Plus SAE 15W-40 delivers value through:One oil for all services, both diesel and gasoline, minimizes the chance of misapplication.educed inventory investment — No need to maintain.. |
|||
Flash Point | 238 °C | 460 °F | ASTM D92 |
ExxonMobil 320 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Flash Point | 238 °C | 460 °F | ASTM D92 |
ExxonMobil 34 Mobil Mist Lube Series Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig.. |
|||
Flash Point | 238 °C | 460 °F | ASTM D92 |
ExxonMobil 680 Mobilgear SHC XMP Series Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin .. |
|||
Flash Point | 238 °C | 460 °F | |
ConocoPhillips Hydroclear® 68 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Flash Point | 238 °C | 460 °F | |
ConocoPhillips Hydroclear® 68 Multipurpose R&O Oil, AGMA Lubricant No. 2 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear .. |
|||
Flash Point | 238 °C | 460 °F | |
ConocoPhillips IGL-9 Enclosed Gear Lubricant ISO 460, AGMA Number 7EP Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service co.. |
|||
Flash Point | 238 °C | 460 °F | ASTM D92 |
ChevronTexaco Delo® 300 Motor Oil, SAE 30 Features:Chevron Delo 300 Motor Oils are high sulfated ash superior “Series 3-type” crankcase oils for four-stroke diesel engines requiring a high detergent crankcase oilThey are manufactured usin.. |
|||
Flash Point | 238 °C | 460 °F | |
ConocoPhillips Hydroclear® 350 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |
|||
Flash Point | >= 238 °C | >= 460 °F | Pensky-Martin closed cup |
ACC EP Primer 28 EPI Engineered Polymers Aromatic polyisocyanate Prepolymer EP Primer 28 is a polyisocyanate prepolymer based on diphenylmethane diisocyanate (MDI). As corrosion-resistant primers, coatings based on EP Primer 28 polyisocyanate can be formulated to contain z.. |
|||
Flash Point | 238 °C | 460 °F | |
ConocoPhillips 1000 Gear Oil AGMA Lubricant No. 8AEP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Flash Point | 238 °C | 460 °F | ASTM D92 |
ExxonMobil 525 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |
|||
Flash Point | 238 °C | 460 °F | |
ChevronTexaco Havoline® SAE 5W-20 Motor Oil All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib.. |