Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 156 °C @Pressure 1.013 MPa |
313 °F @Pressure 146.9 psi |
|
Solvay Chemicals 1,2,3-Trichloropropane Colourless liquid, mainly used as chemical intermediate.EINECS Number: 202-486-1/CAS Number: 96-18-4/UN number: 2810Information provided by Solvay |
|||
Boiling Point | 156 °C | 313 °F | |
BASF Tripropylamine Formula: C9H21NCAS: 102-69-2Description: Tripropylamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water. Synonyms: Propyldi-n-propylamine, Tri-n-propylamine, N,N-Di.. |