Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 165 - 185 °C | 329 - 365 °F | |
Sibur ONZ-40 Compound M-258 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |