Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 740 °C | 1360 °F | |
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Softening Point | 736 °C | 1360 °F | 10<sup>7.6</sup> dPa-s |
Schott D 263 Thin Borosilicate Glass D 263 is a low alkali borosilicate glass that is produced by melting the purest raw materials. As such, it is very resistant to chemical attack. D 263, with its specific properties and large rang.. |
|||
Softening Point | 736 °C | 1360 °F | Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3 |
Schott Glass 8651 Sealing Glass Tungsten sealing glass Power diodesInformation provided by SCHOTT AG. |
|||
Softening Point | 740 °C | 1360 °F | |
Schott S8801 Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |