Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 70.0 °C | 158 °F | Average value: 70.0 °C Grade Count:26 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
Softening Point | 70.0 - 80.0 °C | 158 - 176 °F | Average value: 76.8 °C Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Softening Point | 70.0 °C | 158 °F | ISO 306 |
Iran Petrochemical (PCC) BL2 HF 4750 High Density Polyethylene BL2 is a high density polyethylene with 1-Butene as co monomer. It is high impact strength and slightly, lower stiffness than BL3, outstanding resistance to stress cracking, even in contact with su.. |
|||
Softening Point | 70.0 - 80.0 °C | 158 - 176 °F | MQSA 70A |
Lubrizol Advanced Materials Pearlbond® Eco D900 Thermoplastic Polyurethane Pearlbond™ ECO D900 is a linear, aromatic polyurethane based on specialty polyol from renewable sources. It contains 67% of renewable material as certified according to ASTM-D6866. It is suppli.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Neopor® 2300 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Neopor® 2400 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Neopor® 5300 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Neopor® 5300 Plus Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Peripor® 200 Expandable Polystyrene Description: Expandable polystyrene (EPS) with uniformly distributed flame retardant (blowing agent: pentane)Remarks: Low-pentane products for the production of flame-retardant foams displaying low .. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® F 215 N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing a uniformly distributed ?ame retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foams.Applications: Blocks, insula.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® F 215 T-N Expandable Polystyrene Use: Expanding-agent containing plastic for the production of foam plasticInformation provided by BASF |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® F 315 T-N Expandable Polystyrene Use: Expanding-agent containing plastic for the production of foam plasticsInformation provided by BASF |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® F 315-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkageApplicati.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® F 395 -N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® P 326 M Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded parts with very good mechanical .. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® P 570 Expandable Polystyrene Additive Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: For the production of expanded particles as a filling material .. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Peripor® 300 Expandable Polystyrene Description: Expandable polystyrene (EPS) with uniformly distributed flame retardant (blowing agent: pentane)Remarks: Low-pentane products for the production of flame-retardant foams displaying low .. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® F 215 L-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing a uniformly distributed came retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foams.Applications: Low-density bl.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® F 295-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkageApplicati.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® F 495-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® P 226 C Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Blocks with very short cycle times.Info.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® P 326 C Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded partsInformation provided by BAS.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® P 326 Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded partsInformation provided by BAS.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® P 426 Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts.Information pr.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® P 656 Expandable Polystyrene Additive Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: Filling material for lightweight plasters.Information provided .. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Neopor® 2200 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Neopor® 2400 CT Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Neopor® P 5200 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of silver-gray foams having a considerably higher ther.. |
|||
Softening Point | 70.0 - 80.0 °C | 158 - 176 °F | Kofler; MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® 118 Thermoplastic Polyurethane The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pellet fo.. |
|||
Softening Point | 70.0 °C | 158 °F | approx |
BASF Styropor® P 426 C Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts with very shor.. |