Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 415 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 170 - 213 °C
338 - 415 °F
Average value: 196 °C Grade Count:3
Overview of materials for Polyarylsulfone (PAS), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyarylsulfone; Molded/Extruded". Each property range of values reported is minimum and maximum values ..
Deflection Temperature at 1.8 MPa (264 psi) 204 - 213 °C
400 - 415 °F
Average value: 208 °C Grade Count:13
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E..
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 213 °C
158 - 415 °F
Average value: 193 °C Grade Count:78
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Deflection Temperature at 1.8 MPa (264 psi) 204 - 213 °C
400 - 415 °F
Average value: 208 °C Grade Count:8
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma..
Deflection Temperature at 1.8 MPa (264 psi) 70.0 - 213 °C
158 - 415 °F
Average value: 173 °C Grade Count:4
Overview of materials for Thermoset Polyurethane Foam, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Glass Filled". Each property range of values reported is minimum and maximu..
Deflection Temperature at 1.8 MPa (264 psi) 62.8 - 213 °C
145 - 415 °F
Average value: 136 °C Grade Count:47
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..