Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 48.0 - 51.0 °C
118 - 124 °F
ASTM D648
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer
Somos® NeXT combines stiffness and impact resistance which brings it close the performance of injection molded thermoplastics. It produces finished parts with tight tolerances and detailed features..
Deflection Temperature at 1.8 MPa (264 psi) 35.0 - 51.0 °C
95.0 - 124 °F
ASTM D648
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Deflection Temperature at 1.8 MPa (264 psi) 35.0 - 51.0 °C
95.0 - 124 °F
ASTM D648
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..