Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 42.0 - 49.0 °C | 108 - 120 °F | ISO-R 75 Method A |
Hippe PE 300 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 43.0 - 49.0 °C | 109 - 120 °F | ASTM D648 |
3D Systems Accura® 40 Plastic for SLA® Systems 40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components a.. |