Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 284 °C | 543 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 284 °C | 543 °F | |
MTI ThermoStran® PPA-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 284 °C | 543 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 284 °C @Thickness 3.20 mm |
543 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 284 °C | 543 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI) Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 284 °C | 543 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 284 °C | 543 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |