Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 218 °C | 425 °F | ASTM D648 |
Polymer Resources NY66-IM2-G13-[color]-H Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized Nylon 66, 13% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 °C | 425 °F | 0.125 in; ASTM D 648 |
Matrixx Group 80S7451 45% Glass Reinforced PET
(discontinued **) Data provided by The Matrixx Group, formerly RePlas. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 °C | 425 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/10 GF50 L 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 °C | 425 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6,6 GF33 HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricatedFeatures: LubricatedProcessing Method: Injection MoldingAppearance: .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 °C | 425 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® N340HL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated, Recycled Content Features: Heat stabilizedLubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC 310 Cosmetic and Appliance Grade Compound BMC 310 is a cosmetic and appliance grade material with superior heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical app.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical ap.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC HT12-1026 Unsaturated Polyester Bulk Molding Compound BMC HT12-1026 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC T44-15613 High Strength Mineral Filled Molding Compound BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC 324 Automotive Grade Molding Compound BMC 324 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 324 can be metallized directly, without an initial base-co.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound BMC HT12-1023L is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid cap.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC HT12-1024 Automotive Grade Molding compound BMC HT12-1024 is a high temp wear resistant molding compound designed for automotive brush holders. It is listed under Ford WS-MSD-A. It can be injection or transfer molded.Information provided by.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC T45HT Automotive Grade Molding compound BMC T45HT was designed for the very demanding applications of automotive under hood engine covers. It meets the GMP UP .007 specification for automotive under hood. BMC T45HT is a vinyl ester base.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 218 - 260 °C | 425 - 500 °F | |
Bulk Molding Compounds BMC T70 Automotive Grade Molding compound BMC T70 is a low profile automotive grade molding compound specifically formulated for the vacuum metallization process. These compounds have excellent physical properties as well as superior adhes.. |