Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 330 °F | |
Greene Tweed Arlon® 1330 PEEK Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 330 °F | ASTM D648 |
Techmer ES Electrafil® J-80/CF/20 NAT Acetal (POM) Copolymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 330 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® POM CO GF/M30 UV BK 30% Glass Milled/Glass Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Milled/Glass Fiber, 30% Filler by WeightAdditive: UV StabilizerFeatures: Copolymer and Chemically CoupledAppearance: BlackInforma.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 330 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® POM CO GF25 CC 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 25% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 330 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA12 GF50 L 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 166 °C | 330 °F | ASTM D648 |
Westlake Plastics PEEK Film Made from VICTREX® Polymer Extremely high temperature resistance and continuous use temperature. Excellent flexural and tensile properties. Good abrasion and rain erosion resistance. Excellent chemical resistance. Excelle.. |