Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 143.0 °C | 289.4 °F | Unannealed, 0.062 in bars; ASTM D648 |
PolyOne Therma-Tech™ NJC-5000 TC NATURAL Nylon 12
(discontinued **) Information provided by PolyOne Corporation. |